Loading…
Loading…
| # | Company | Quoted % | Amount | Rank | Status |
|---|---|---|---|---|---|
| 1 | L1₹9.9 LAdmitted-Finance | -0.27% | ₹9.9 L | L1 | Admitted-Finance |
Tender Value
₹9.9 L
EMD Value
₹19,757
Closing Date
22 Jan 2026, 6:00 pmClosed
DPC, SAMAGRA SHIKSHA JODHPUR
DPC, SAMAGRA SHIKSHA JODHPUR
Bhopalgarh Cluster-7 ARTIYA KALLAN 153, ARTIYA KALLAN 154, ARTIYA KHURD 155, ARTIYA KHURD 156, BANDRA 158, BUDAKIYA 160, BUDAKIYA 161, GULAI NADI 179, SHIV NAGAR 165, VISHNU NAGAR 164, NANDIYA 162, NANDIYA 163, DEVTDA 172, DEVATDA 174, DEVATDA 173,
2026_RCSCE_529676_8
nit-30/civil/adpc-jodh./25-26
Open Tender
Civil Works
60 days
adpc jodhpur
Please refer Tender documents.
2 documents required · 2 mandatory
₹1,000
Yes
DPC, SAMAGRA SHIKSHA JODHPUR AND MD RISL JAIPUR
₹19,757
Yes
23 Jan 2026
20 Jan 2026
23 Jan 2026
20 Jan 2026
22 Jan 2026
20 Jan 2026
(Aanganwadi GAJSINGHPURA 14) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi GAJSINGHPURA 15) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi GAJSINGHPURA 16) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi GAJSINGHPURA 19) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi MANGERIYA 37) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi MANGERIYA 38) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi ANWALO KI DHANI 41) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi DHANDORA 36) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi TODIYAL 39) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi RADOD 20) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi RADOD 22) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi LAWARI 18) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi ASANDA 17) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi KUMABHARA 76) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi SURPURA 70) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi SURPURA 71) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi SEKHNIYAWAS 75) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi KUMABHARA 77) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi BHAWANIYA NAGAR 74) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi HINGOLI 72) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
(Aanganwadi BASNI HARISINGH 49) Dismantling stone slab/ terrazo chip flooring laid in cement mortar including stacking of serviceable material and disposal of unserviceable material within 50 meters lead. Cement Concrete Roofing
Grading roof for water proofing treatment with water proffing compound Cement concrete 1:2:4 (1 cement : 2 coarse sand : 4 graded stone aggregate 20 mm nominal size)
Coping:Cement concrete flooring grade 1:2:4 (1-Cement:2-Coarse sand:4-graded stone aggregate) rounding off edges etc. but excluding the cost of nosing of steps etc. complete : 50 mm thick with 20 mm thick nominal size aggregate.
Providing batta (gola) 75mm x 75mm in cement concrete (1:2:4) including finished with cement mortar 1:3 as per standard design.
Providing & laying broken glazed titles on roof ( broken glazed tiles not less than 9 Kg/Sqm) on top of hot bitumen @ 1.7 Kg/Sqm. (1.40 Kg of VG-40 (30/40 )grade and 0.30 Kg/Sqm. Of VG-10 (80/100) grade) and joints filled with cement mortar 1 :2 (1 cement:2 marble dust mixed with water proofing compund all complete as per direction of Engineer-in-charge.
Please Enable Macros to View BoQ information
stage.html
html • 0.02 MB
tech_eval.pdf
boq_comp_chart.xlsx
xlsx
Tap a document below to read it instantly. You can also download everything as a ZIP if you prefer.
details.html
html • 0.03 MB
Tendernotice_1.pdf
PDF • 3.38 MB
BOQ_944595.xls
BOQ • 0.40 MB
Download all tender documents and submit your bid